详细说明 Thermanit 25/35 R Classifications EN 1600 Mat. No. E Z25 35 Nb B 2 2 1.4853 说明: Resistant to scaling up to 1050 °C (1922 °F). For surfacing and joining work on matching/similar heat resistant cast steel grades. 对扩大到1050°C(1922°F)。 堆焊和加入工作匹配/类似的热 耐铸钢的成绩。 用途: TüV certified parent metal GX40NiCrNb35-25 (1.4852) 熔敷金属化学成分(%)C Si Mn Cr Ni Nb 0.40 1.0 1.8 25.0 35.0 1.3 熔敷金属力学性能Heat- Yield strength Yield strength Tensile Elongation treatment 0.2% 1.0% strength (L0=5d0) N/mm2 N/mm2 N/mm2 % AW 400 450 600 8 参考电流 (AC、DC+)Packaging, weights and amperages Dimensions (mm) pcs./pack kg/pack Amperage A 2.5 x 300 210 3.8 55- 80 3.2 x 350 130 4.2 80-105 4.0 x 350 94 4.6 90-135