详细说明 Thermanit 625 Basic covered electrode C Si Mn Cr Mo Ni Nb Fe <0.04 <0.7 <1 21.5 9.5 Bal. 3.3 <2.0 Characteristics and field of use Materials Typical analysis in % TüV certified parent metals X10NiCrAlTi32-20 H, X10NiCrAlTi32-20 (1.4876), NiCr22Mo9Nb (2.4856), X2NiCrMoCu25-20-5 (1.4539), X2CrNiMoCuN20-18-6, VdTüV-WBL. 473; Alloy 600, Alloy 625, Alloy 800, 9% Ni steels Stainless; high resistance to corrosive environments. Resistant to stress corrosion cracking. Resistant to scaling up to 1100 °C (2012 °F). Temperature limit: 500 °C (932 °F) max. in sulphureous atmospheres. High temperature resistant up to 1000 °C (1832 °F). Cold toughness at subzero temperatures as low as –196 °C (–321 °F). For joining and surfacing work with matching/similar corrosion resistant materials as well as on matching and similar heat resistant, high temperature steels and alloys. For joining and surfacing work with cryogenic austenitic CrNi(N) steels/cast steel grades and on cryogenic Ni steels suitable for quenching and tempering. 不锈钢,高耐腐蚀性环境。耐药 应力腐蚀开裂。对扩大到1100°C (2012°F)。温度限制:500°C(932°F)马克斯。在 含硫的大气。耐高温 1000°C(1832°F)。寒冷的韧性在零下的温度 低至-196°C(-321°F)。加入,忽而工作 与匹配/以及类似的耐腐蚀材料 匹配和相似的耐热,耐高温钢 和合金。加入,忽而使用低温 奥氏体CrNi(N)钢/铸钢成绩和低温 镍钢适合淬火及回火。